Growth of single-walled carbon nanotube (SWCNT) was achieved by an alcohol catalytic chemical vapor deposition (CVD) mechanism that was conducted in a high vacuum using Ru catalysts. By optimizing the ethanol pressure, SWCNTs can grow in a wide range of temperature between 500 °C and 900 °C. Both the yield and crystalline quality of SWCNTs reached their maxima at 700 °C. Significantly, the SWCNT growth was achieved even at 450 °C, which was much lower than the growth temperatures that were required for SWCNT growth using Ru catalysts previously. Raman measurements exhibited that the diameter distribution of the SWCNTs that were grown at 450 °C was quite narrow and (11, 4) nanotubes were dominant. The observations of transmission electron microscope (TEM) suggested that the size of the Ru particles were larger than the diameter of SWCNT. Such a relation was similar to the relation observed in the growth of SWCNTs using Pt catalysts.
Full text views reflects PDF downloads, PDFs sent to Google Drive, Dropbox and Kindle and HTML full text views.
* Views captured on Cambridge Core between 10th January 2018 - 8th March 2021. This data will be updated every 24 hours.
Please note a has been issued for this article.