Characterization of the Electrical Properties of Nickel-Based CMSX-4 Super-alloys Using Atomic Force Microscopy (AFM)

Published online by Cambridge University Press:  01 August 2004

Guangchun Cui
Affiliation:
Georgia Institute of Technology
Rosario A Gerhardt
Affiliation:
Georgia Institute of Technology
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2004 in Savannah, Georgia, USA, August 1–5, 2004.