Microstructure of (Y + Sm)–α-sialon with a-sialon seeds

Published online by Cambridge University Press:  31 January 2011

Wei-wu Chen
Affiliation:
The State Key Lab of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Shanghai 200050, People's Republic of China
Wei-ying Sun
Affiliation:
The State Key Lab of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Shanghai 200050, People's Republic of China
Ya-wen Li
Affiliation:
The State Key Lab of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Shanghai 200050, People's Republic of China
Dong-sheng Yan
Affiliation:
The State Key Lab of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Shanghai 200050, People's Republic of China
Get access

Abstract

(Y + Sm)–α-sialon compositions with and without α-sialon seeds were hot-pressed at 1800 °C for 1 h and then heat treated at 1800 °C for 4 h. The effect of α-sialon seeds on the microstructures of (Y + Sm)–α-sialon ceramics was studied by scanning electron microscopy. The results showed that hot-pressed α-sialon ceramics with elongated grains can be fabricated by adding 10 wt% seeds. Through heat treatment, the seed-free composition could also develop into a similar microstructure with big elongated grains dispersed in a fine matrix.

Type
Articles
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Becher, P.F., J. Am. Ceram. Soc. 74, 255 (1991).CrossRefGoogle Scholar
2. Cao, G.Z. and Metselaar, R., Chem. Mater. 3, 242 (1991).CrossRefGoogle Scholar
3. Chen, I-Wei and Rosenflanz, Anatoly, Nature 389, 701 (1997).CrossRefGoogle Scholar
4. Zhao, H., Swenser, S., and Cheng, Y.B., J. Eur. Ceram. Soc. 18, 1053 (1998).CrossRefGoogle Scholar
5. Shen, Z.J., Nordberg, L.O., Nygren, M., and Er, T.?ström in Engineering Ceramics '96: Higher Reliability through Processing, edited by Babini, G.N. et al. (Kluwer Academic Publishers, Dorbrecht, The Netherlands, 1997), p. 169.CrossRefGoogle Scholar
6. Mitomo, M., Key Eng. Mater. 161–163, 53 (1999).Google Scholar
7. Zhang, C., Sun, W.Y, and Yan, D.S., J. Eur. Ceram. Soc. 19, 33 (1999).CrossRefGoogle Scholar
8. Wang, P.L., Sun, W.Y., and Ten, T.S., Eur. J. Solid State Inorg. Chem. 31, 93 (1994).Google Scholar
9. Petzow, G. and Hoffmann, M.J., Mater. Sci. Forum 113–115, 91 (1993).CrossRefGoogle Scholar
10. Kingery, W.D., Bowen, H.K., and Uhlmann, D.R., (John Wiley & Sons, New York, 1976), p. 451.Google Scholar
11. Kim, Y-W., Mitomo, M., and Hirotsurn, H., J. Am. Ceram. Soc. 80, 99 (1997).CrossRefGoogle Scholar
12. Kang, S-J.L and Han, S-M., MRS Bull. 2, 3336 (1995).Google Scholar
13. Chen, W.W., Sun, W.Y., Li, Y.W., and Yan, D.S., Mater. Lett. (2000, in press).Google Scholar