3 - Single-crystal superalloys for blade applications

Published online by Cambridge University Press:  01 September 2009

Roger C. Reed
Affiliation:
Imperial College of Science, Technology and Medicine, London
Get access

Summary

The gas turbine consists of many different pieces of turbomachinery, but the rows of turbine blading are of the greatest importance since many engine characteristics, for example the fuel economy and thrust, depend very strongly on the operating conditions which can be withstood by them. Thus very arduous temperatures and stresses are experienced by the materials employed, which are pushed near to the limits of their capability. This is particularly the case for the high-pressure blades, which are located nearest to the hot gases emerging from the combustion chamber. Their function is to extract work from the gas stream and to convert it to mechanical energy in the form of a rotating shaft, which drives the high-pressure compressor.

A consideration of the operating conditions experienced by the high-pressure turbine blades in a large civil turbofan engine, such as the Rolls-Royce Trent 800 or General Electric GE90, confirms this point. The temperature of the gas stream is about 1750 K, which is above the melting temperature of the superalloys from which the blades are made. The high-pressure shaft develops a power of about 50 MW – hence, with about 100 blades, each extracts about 500 kW, which is sufficient to satisfy the electricity requirement of about 500 homes. Each row of blades is expected to last at least 3 years, assuming they operate at 9 h/day. This is equivalent to about 5 million miles of flight, or ~500 circumferences of the world.

Type
Chapter
Information
The Superalloys
Fundamentals and Applications
, pp. 121 - 216
Publisher: Cambridge University Press
Print publication year: 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Save book to Kindle

To save this book to your Kindle, first ensure coreplatform@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

Available formats
×