Summary

Overview

Stress corrosion, or stress corrosion cracking (SCC), and fatigue/corrosion fatigue, or fatigue crack growth (FCG), are problems of long standing. They manifest themselves in the occurrence of “delayed failure” (i.e., failure after some period of time or numbers of loading cycles) of structural components under statically or cyclically applied loads, at stresses well below the yield strength of the material. These phenomena of delayed failure are often referred to as “static fatigue,” for SCC, or simply “fatigue” for cyclically varying loads. The traditional measure of stress corrosion cracking susceptibility is given in terms of the time required to produce failure (time-to-failure) at different stress levels, as obtained from testing “smooth” or “notched” specimens of the material in the corrosive environments (for example, sea water, for marine applications). For fatigue, the measure is given by the number of cycles to cause failure (the fatigue life) at given cyclic stress levels, or the endurance limit (stress corresponding to some prescribed number of load cycles; e.g., 106 cycles).

The failure time, however, incorporates both the time required for “crack initiation” and a period of slow crack growth so that the separate effect of the environment on each of these stages cannot be ascertained. (Some of the difficulty stems from the lack of a precise definition for crack initiation.) This difficulty is underscored by the results of Brown and Beachem on SCC of titanium alloys.

Type
Chapter
Information
Fracture Mechanics
Integration of Mechanics, Materials Science and Chemistry
, pp. 103 - 119
Publisher: Cambridge University Press
Print publication year: 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Brown, B. F. and Beachem, C. D., “A Study of the Stress Factor in Corrosion Cracking by use of the Pre-cracked Cantilever Beam Specimen,” Corrosion Science, 5 (1965), 745–750.CrossRefGoogle Scholar
Wei, R. P., “Application of Fracture Mechanics to Stress Corrosion Cracking Studies,” in Fundamental Aspects of Stress Corrosion Cracking, NACE, Houston, TX (1969), 104.
Wei, R. P., Novak, S. R., and Williams, D. P., “Some Important Considerations in the Development of Stress Corrosion Cracking Test Methods,” AGARD Conf. Proc. No. 98, Specialists Meeting on Stress Corrosion Testing Methods, 1971, Materials Research and Standards, ASTM, 12, 9 (1972), 25.Google Scholar
Wei, R. P., “Fracture Mechanics Approach to Fatigue Analysis in Design,” J. Eng'g. Mat'l. & Tech., 100 (1978), 113–120.CrossRefGoogle Scholar
Williams, D. P., and Nelson, H. G., “Gaseous Hydrogen – Induced Cracking of Ti-5Al-2.5Sn,” Met. Trans., 3, 8 (1972), 2107.CrossRefGoogle Scholar
Chu, H. C., and Wei, R. P., “Stress Corrosion Cracking of High-Strength Steels in Aqueous Environments,” Corrosion, A6, 6 (1990), 468–476.CrossRefGoogle Scholar
Harter, J., ARGROW Program; AFGROW/VASM, http://www.stormingmedia.us/13/1340/A134073.html, (2004).
Newman, J. C., “FASTRAN II – A fatigue crack growth structural analysis program,” NASA TM-104159 (1992).
Thomas, J. P., and Wei, R. P., “Standard-Error Estimates for Rates of Change from Indirect Measurements”, Technometrics, 38,1 (1996), 59–68.CrossRefGoogle Scholar

Save book to Kindle

To save this book to your Kindle, first ensure coreplatform@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

Available formats
×